Notice: Function _load_textdomain_just_in_time was called incorrectly. Translation loading for the wordpress-seo domain was triggered too early. This is usually an indicator for some code in the plugin or theme running too early. Translations should be loaded at the init action or later. Please see Debugging in WordPress for more information. (This message was added in version 6.7.0.) in /var/www/html/wp-includes/functions.php on line 6260 Corrective Aqua Concealer Stick - Happi
Color Cosmetics, Skin Care

Corrective Aqua Concealer Stick

Released By Lubrizol

Corrective Aqua Concealer Stick
Ingredients
%

Phase A

  • Water (Deionized water)
  • 10.70
  • Butylene glycol
  • 3.00
  • Phenoxetol (Clariant) (Phenoxyethanol)
  • 0.30
  • Eyeseryl Peptide Solution (Lipotec SAU) (Water (and) butylene glycol (and) acetyl tetrapeptide-5)
  • 5.00
  • Avalure Flex-6 Polymer (Lubrizol Advanced Materials) (Polyurethane-62 (and) trideceth-6)
  • 1.00

Phase B

  • Schercemol NGDO Ester (Lubrizol Advanced Materials) (Neopentyl glycol diethylhexanoate)
  • 29.25
  • Schercemol DID Ester (Lubrizol Advanced Materials) (Diisopropyl dimer dilinoleate)
  • 10.00
  • Unipure White LC 987 AS-EM (Sensient) (CI 77891 (and) triethoxycaprylylsilane)
  • 13.75
  • Unipure Yellow LC 182 AS-EM (Sensient) (CI 77492 (and) triethoxycaprylylsilane)
  • 1.60
  • Unipure Red LC 381 AS-EM (Sensient) (CI 77491 (and) triethoxycaprylylsilane)
  • 0.50
  • Unipure Black LC 989 AS-EM (CI 77499 (and) triethoxycaprylylsilane)
  • 0.15
  • RonaFlair Boroneige SF-6 (Merck KGaA) (Boron nitride)
  • 4.00
  • RonaFlair LDP White (Merck KGaA) (Titanium dioxide (and) sodium potassim aluminium silicate (and) tin oxide)
  • 1.00
  • EL-8051 IN Silicone Organic Elastomer Blend (Dow Corning) (Isodecyl neopentanoate (and) dimethicone/bisisobutyl PPG-20 crosspolymer)
  • 3.00

Phase C

  • Cerozo RS HA/C (Baerlocher) (Ozokerite)
  • 11.00
  • Kahlwax 2811 (Kahlwax) (Oryza sativa (rice) bran wax)
  • 4.00

Phase D

  • Vitamine E Acetate (Tocopheryl acetate)
  • 0.50
  • Allergen Free Aloe Vera (Sensient) (Fragrance)
  • 0.25
  • Xiameter PMX-200 5 cs (Dow Corning) (Dimethicone)
  • 1.00

Procedure

Weigh the ingredients of part A except the Avalure Flex-6 polymer and heat to 50°C, then add slowly Avalure Flex-6 polymer until complete dispersion then raise the temperature to 90°C (it can prepared the day before). Add part B ingredients one at a time in a suitable vessel under homogenizer at 3000 rpm for 10 minutes while heating to 100°C. Weigh part C and heat it to 100°C. Add part B to part C then add the ingredients of part D. Make the emulsion by quickly adding part B/C/D to part A at 600 rpm. Keep the bulk at 90°C until emulsion is completed. Fill the pre-heated and siliconed molds.

Properties

Appearance—Beige stick; Stability—Passed 1 month @ 50°C, 40°C, 4°C and 25°C and 5 freeze/thaw cycles; Avalure Flex-6 Polymer (wt% TS)—1.00

More Information

Lubrizol Tel: 800-379-5389 or 216-447-5000 Website: www.lubrizol.com/personal-care

Request more information from Lubrizol